Fabricating Debris – Audible Test – Fix Scratched Glass

Sunday, February 17th, 2013

Fabricating debris can be removed before it scratches!

 

Fabricating debris is the invisible glass scratching menace!  When the slider right next to this one was badly scratched in the same pattern as the window washer used when scraping all the constructing junk off, we check this one for fabricating debris from the tempering process.  Of course it was there but the interesting thing was that we normally sand and polish but we have been experimenting with a one step fabricating debris removal process which shows some real promise. Look and listen.

Fabricating debris closeup

Sample fabricating debris scratches on tempered glass Riverhead NY

 

Fabricating debris – Closeup

This is actually very big news. The fact that we were able to remove the scratch causing fabricating debris before it has scratched the glass saves lots of time over sanding and polishing.  While we do still have the fastest glass resurfacing process, this continues to make our advancements in glass restoration even more pronounced.  If you discover this menacing debris on your glass surface, call us and we can assist you in turning this low quality glass into premium, totally clear, scratch free glass while removing all the scratch causing debris.

  Previous                                                                                                                                            Next 

Scratched Tempered Glass Curtain Wall Resurfacing Begins 6-7-2010 Biloxi, MS

Friday, June 4th, 2010

Things have finally progressed.  We will be tackling a 7000+ sq. ft. curtain wall of tempered dual pane impact glass in Biloxi, MS.  We should be able to complete the massive scratched glass repair project within 3 weeks.